747 Cobalt Stick Rod Electrode, 38 to 42 HRC Hardness, 110 to 165 Amps, AC/DCRP Polarity, Corrosion Resistance, 5/32"
(Pack of
5)
SKU:CW1833 Item#: CW1833
A selection of alloys to meet specialty wear or hardfacing needs. High frictional wear resistance for most ferrous and non-ferrous metals
Cobalt alloy formulated for hardness, corrosion resistance and stability at temperatures up to 2,000°F (1,093°C)
Compressive Strength: To 230,000 PSI
Hardness: Up to Rc 42, work-hardened
Polarity: AC or DC Straight or Reverse
Usage ProcedureUtilizing a little longer arc than normal (about 1/8" 5/32") will promote smooth arc transfer, avoiding slag entrapment and short-circuiting. Stringer beads are usually recommended to avoid slag inclusions. Position the electrode perpendicular to the surface to promote coating melt to core wire balance. Straight polarity achieves less base metal dilution.
Frequently Bought Together
172 Intermediate Abrasion And Impact Alloy 5/32X18
Couldn't load pickup availability
711 Carbide Hard Facing Stick Rod Electrode 5/32"
Couldn't load pickup availability
281 Martensitic Stick Rod Electrode 1/8"
Couldn't load pickup availability
Utility Knife, Folding , 4" Closed
Couldn't load pickup availability
USS Flat Washer Thru-Hardened Steel 3/8"
Couldn't load pickup availability
SAE Flat Washer Thru-Hardened Steel 5/16"
Couldn't load pickup availability
747 Cobalt Stick Rod Electrode 1/8"
Couldn't load pickup availability
Round Soapstone 1/4 x 5"
Couldn't load pickup availability
331 Mild and Carbon Steel MIG Welding Wire 0.03"
Couldn't load pickup availability
321 Mild and Carbon Steel MIG Welding Wire 0.035"
Couldn't load pickup availability
Product Description
A selection of alloys to meet specialty wear or hardfacing needs. High frictional wear resistance for most ferrous and non-ferrous metalsCobalt alloy formulated for hardness, corrosion resistance and stability at temperatures up to 2,000°F (1,093°C)
Compressive Strength: To 230,000 PSI
Hardness: Up to Rc 42, work-hardened
Polarity: AC or DC Straight or Reverse
Usage ProcedureUtilizing a little longer arc than normal (about 1/8" 5/32") will promote smooth arc transfer, avoiding slag entrapment and short-circuiting. Stringer beads are usually recommended to avoid slag inclusions. Position the electrode perpendicular to the surface to promote coating melt to core wire balance. Straight polarity achieves less base metal dilution.
Technical Specifications
| Item#: | CW1833 |
|---|---|
| Welding Process | Stick |
| Diameter | 5/32 " |
| Base Metal | Cobalt |
| Hardness | 38-42 HRC |
| Polarity | AC/DCRP |
| UNSPSC #: | 23271810 |
| TAA Compliant: | Yes |
| Weight: | 5.0 lb |