30 Copper and Steel Flux Coated Brazing Rod, Pink, 18" Length, 3/32"
(Pack of
5)
SKU:CW1006 Item#: CW1006
A selection of brazing alloys for joining cast iron and brazing sheet metal.
Superior Advantages
Solid, dense deposits that can be machined
Free-flowing for thin lapping and butted metal joining
No base metal dilution making tough cast iron repairs possible
Maximum strength for joining and buildup
Flux Coating Color: PinkTensile Strength: 100,000 PSITemperature: 1,300°F to 1,600°F (704°C to 871°C)Recommended Flux: F21 (if needed)
Typical Applications
Sheet metal and auto body repairs
Engine heads and blocks
Piping, plumbing and pumps
Gears, sprockets and pulleys
Usage ProcedureClean joint areas thoroughly. Heat metal with neutral flame until flux liquifies. Base metals should be dull red as Cronabraze™ 30F commences to penetrate the joint. Use rapid weaving motion with torch to deposit alloy drop-by-drop. Do not concentrate heat enough to melt base metal. Remove flux residue with water.
Couldn't load pickup availability
California Proposition 65: WARNING: Cancer -
www.P65Warnings.ca.gov
Catalog page#: 13-29
Frequently Bought Together
41 Silver Flux Coated Brazing Rod 1/16"
Couldn't load pickup availability
46 Sil-Phos Bare Brazing Rod 1/8"
Couldn't load pickup availability
54 Medium Silver Flux Coated Brazing Rod 1/16"
Couldn't load pickup availability
Hex Nut Grade 8 Alloy Steel 1/4-20
Couldn't load pickup availability
Superbutt Connector 16 to 14 AWG Blue
Couldn't load pickup availability
SAE Flat Washer Thru-Hardened Steel 5/16"
Couldn't load pickup availability
30 Copper and Steel Flux Coated Brazing Rod 1/16"
Couldn't load pickup availability
Oxy-Therm Cutting Rod 3/8 x 24"
Couldn't load pickup availability
Rosin Core Solder 0.032"
Couldn't load pickup availability
Round Soapstone 1/4 x 5"
Couldn't load pickup availability
Product Description
A selection of brazing alloys for joining cast iron and brazing sheet metal.Superior Advantages
Solid, dense deposits that can be machined
Free-flowing for thin lapping and butted metal joining
No base metal dilution making tough cast iron repairs possible
Maximum strength for joining and buildup
Flux Coating Color: PinkTensile Strength: 100,000 PSITemperature: 1,300°F to 1,600°F (704°C to 871°C)Recommended Flux: F21 (if needed)
Typical Applications
Sheet metal and auto body repairs
Engine heads and blocks
Piping, plumbing and pumps
Gears, sprockets and pulleys
Usage ProcedureClean joint areas thoroughly. Heat metal with neutral flame until flux liquifies. Base metals should be dull red as Cronabraze™ 30F commences to penetrate the joint. Use rapid weaving motion with torch to deposit alloy drop-by-drop. Do not concentrate heat enough to melt base metal. Remove flux residue with water.
Technical Specifications
| Item#: | CW1006 |
|---|---|
| Welding Process | Brazing |
| Type | Flux Coating |
| Diameter | 3/32 " |
| Length | 18 " |
| Tensile Strength | 100,000 PSI |
| Melting Temperature | 1560 - 2000 °F |
| Color | Pink |
| Base Metal | Copper/Steel |
| Recommended Flux | F21 |
| Description | All Purpose |
| UNSPSC #: | 23271804 |
| TAA Compliant: | No |
| Weight: | 5.5 lb |
Product Restrictions
California Proposition 65: WARNING: Cancer -
www.P65Warnings.ca.gov